This title is printed to order. This book may have been self-published. If so, we cannot guarantee the quality of the content. In the main most books will have gone through the editing process however some may not. We therefore suggest that you be aware of this before ordering this book. If in doubt check either the author or publisher’s details as we are unable to accept any returns unless they are faulty. Please contact us if you have any questions.
In this work Atomic Layer deposition of niobium and titanium doped ZnO based Transparent Conductive Oxide (TCO) coatings were developed. The fundamentals required for the deposition and doping of ZnO TCOs are discussed. The various opto-electronic properties of the niobium and titanium doped ZnO films were determined and compared. A model was proposed to explain the various changes in the opto-electronic properties of these films.
$9.00 standard shipping within Australia
FREE standard shipping within Australia for orders over $100.00
Express & International shipping calculated at checkout
This title is printed to order. This book may have been self-published. If so, we cannot guarantee the quality of the content. In the main most books will have gone through the editing process however some may not. We therefore suggest that you be aware of this before ordering this book. If in doubt check either the author or publisher’s details as we are unable to accept any returns unless they are faulty. Please contact us if you have any questions.
In this work Atomic Layer deposition of niobium and titanium doped ZnO based Transparent Conductive Oxide (TCO) coatings were developed. The fundamentals required for the deposition and doping of ZnO TCOs are discussed. The various opto-electronic properties of the niobium and titanium doped ZnO films were determined and compared. A model was proposed to explain the various changes in the opto-electronic properties of these films.